pl explain what is function of each alloying elements given below in CSEF steel
Mo,W,Re, V,Nb,Ti,Ta,C & N
Pandithan
 
Other than Re, to develop precipitates that provide elevated temperature tensile strength and creep strength in Grade 91, 92, 23 and 24 alloys.
 