Alloy690 tube to SA516Gr.70 header tig welding consumable

Status
Not open for further replies.

krishh07

Mechanical
Joined
Dec 7, 2014
Messages
16
Location
IN
Dear,

Can any one sugest Alloy690 tube to SA516Gr.70 header tig welding consumable
 
ERNiCr-3 (Filler Metal 82) is readily available and fairly robust when joining nickel alloys to carbon steel.
 