Aug 22, 2013 #1 tekari123 Mechanical Joined Aug 7, 2013 Messages 29 Location IN Dear All, Can a welder weld SA 335 GR P-11 with SA335 GR P22 Filler.. if so, what is the referencing code section? Pl. help Alok
Dear All, Can a welder weld SA 335 GR P-11 with SA335 GR P22 Filler.. if so, what is the referencing code section? Pl. help Alok
Aug 22, 2013 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US Yes, as long as there is a qualified WPS for doing so. It's F-No that's the essential variable for Welder Qualification - not A-No. Upvote 0 Downvote
Yes, as long as there is a qualified WPS for doing so. It's F-No that's the essential variable for Welder Qualification - not A-No.
Aug 22, 2013 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Most Codes and Standards do not recommend filler metals for weld joints, that is left up to the designer. Upvote 0 Downvote