Hallo guys,
i have a code issue problem and would need your help.
This material has a ultimate tensile strength of 490 [MPa] @ 20°C and a yield strength of 355 [MPa] @ 20°C.
Now for the allowable stress according B31.3 2016 does chapter 302.3.2 (d)(1),(2) apply or 302.3.2 (f)?
What is the correct allowable stress:
We use: 0,92 * [max [(490/3),(355/1,5)]] = 150 MPa for sutructural grade materials = 490*0,92/3
or is it only 355/1,5 = 237 MPa
In my opinion 302.3.2 (d)(1),(2) does apply with tensile strength allowable
Thank you and best regards, Stefan
i have a code issue problem and would need your help.
This material has a ultimate tensile strength of 490 [MPa] @ 20°C and a yield strength of 355 [MPa] @ 20°C.
Now for the allowable stress according B31.3 2016 does chapter 302.3.2 (d)(1),(2) apply or 302.3.2 (f)?
What is the correct allowable stress:
We use: 0,92 * [max [(490/3),(355/1,5)]] = 150 MPa for sutructural grade materials = 490*0,92/3
or is it only 355/1,5 = 237 MPa
In my opinion 302.3.2 (d)(1),(2) does apply with tensile strength allowable
Thank you and best regards, Stefan