I have to design tank. Design temperature minus204 to plus 46 degree Celsius. material is SA240 GR 304L. code is ASME SEC. VIII DIV1. I have 2 questions :
1)please guide whether Allowable stress which I have to use for calculating thickness is to be taken that of plus 46 degree Celsius. This is based on my interpretation of following code para.
UHA-23 MAXIMUM ALLOWABLE STRESS
VALUES
((c) For vessels designed to operate at a temperature
below −20°F (−30°C), the allowable stress values to be
used in design shall not exceed those given in Table 1A
or 3 of Section II, Part D for temperatures of −20°F
to 100°F (−30°C to 40°C).
2) when we have maximum & minimum design temperatures, which is to be considered for knowing the allowable stress?
1)please guide whether Allowable stress which I have to use for calculating thickness is to be taken that of plus 46 degree Celsius. This is based on my interpretation of following code para.
UHA-23 MAXIMUM ALLOWABLE STRESS
VALUES
((c) For vessels designed to operate at a temperature
below −20°F (−30°C), the allowable stress values to be
used in design shall not exceed those given in Table 1A
or 3 of Section II, Part D for temperatures of −20°F
to 100°F (−30°C to 40°C).
2) when we have maximum & minimum design temperatures, which is to be considered for knowing the allowable stress?