Allowable Hydrotest stress

Status
Not open for further replies.

kyong

Mechanical
Aug 15, 2001
73
Can anyone tell how allowable hydrotest stress should be determined for flat heads or tubesheets?
 
Replies continue below

Recommended for you

not sure what you are meaning..can you explain a bit more what you are looking for..AYBEE
 
Aybee,

Thank you for your response.

When you perform a hydrotest, you can't apply too high pressure because the stress developed may be excessive. My question is during hydrotest, how high stress can be allowed. On what rule, should the maximum allowable hydrotest stress for flat heads or tubesheets be determined?

kyong
 
ASME VIII Div.2 gives a limit of 90% of min.yield stress for general primary membrane stresses and of 135% of yield for primary membrane plus bending stresses.

prex

Online tools for structural design
 
prex,

Thank you very much.

kyong
 
The ASME codes(fired and unfired pressure vessels) will show you the formulae needed to calculate the MAWP's of these item you mentioned. The hydrostatic test will be at 150% MAWP.
 