Does it really require, if a cylindrical object is welded on a plate (or with a cylindrical object) to give all around weld?
Isn't it implicit?
Is there any discussion about this in the ASME weld standards?

AnandaBalan Devaraji
Product Design Engineer
Tata Consultancy Services
 
Excerpt from ANSI/AWS A2.4-98, "Standard Symbols for Welding, Brazing, and Nondestructive Examination", para. 3.10.2 (page 7):

"3.10.2. Circumferential welds. Weld extending around the circumference of a pipe are excluded from the requirement regarding changes in direction and do not require the weld-all-around symbol to specify continouos weld."
 
I believe that example is for a fluid containing hollow cylinder joined to another fluid containing hollow cylinder. For other configurations, you definitely need to state if a full circumferential weld is necessary or if segments are allowable.
 
Rule 1 is make your drawings clear.

"Implicit" = ambiguous.

The fact that you had to ask goes to show the possibility for misunderstanding.

No one will not understand "all around" in your example.
 
Thanks for your replies.