Apr 23, 2012 #1 WeldUK Materials Joined Jan 20, 2012 Messages 21 Location GB Can anyone recommend a consumable grade?
Apr 23, 2012 1 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US With little other information to go on as to application and environment, use E/ER 410NiMo Upvote 0 Downvote
Apr 23, 2012 1 #3 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US If service parametrs permit, E/ER 309 might also be used. Upvote 0 Downvote
Apr 24, 2012 Thread starter #4 WeldUK Materials Joined Jan 20, 2012 Messages 21 Location GB Thanks everyone for the advice, I am in your same position, no details whatsoever on the service conditions but still asked to provide an answer! Upvote 0 Downvote
Thanks everyone for the advice, I am in your same position, no details whatsoever on the service conditions but still asked to provide an answer!