Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AISC Greenbook designation - Concrete Mixes 1

Status
Not open for further replies.

rscott

Computer
Joined
Feb 13, 2002
Messages
7
Location
US
I am performing a project that requires addition of metric measurements to standards that now are all US.

The concrete mix designs are per AISC greenbook - in the form:

520-C-2500 (520=lb cement "c"=aggrgate size 2500=psi).

The new designation will be metric in the form (I found this formula in a municipality requirement):

310 kg/M(cubed) C 20 MPa

My question is, the conversions do not seem right.

First, I don't know what the M(cubed) is, so I don't know how to crank it in.

Secondly, 2500 psi does not convert to 20 MPa (megpascal).

I may be way off base, and am unfamiliar with this discipline.

Can anyone help clarify for me? Thanks so much...
 
hi rscott,

Your first question is simple, and the conversion is correct. M(cubed) is someone's representation of 'cubic metre'.

The 520 is pounds per cubic yard. At 1 cubic metre = 1.307 cubic yards, and 1 kg = 2.2046 pounds, you get 520*1.307/2.2046=308 kg/m^3. Round up to 310.

Your second comment is quite valid. 2500 psi converts to 2500/145.04=17.2 MPa. To round that up to 20 MPa seems like some dog-rough science to me. I would not be party to calling that a 20 MPa mix.
 
Thank you for your informative and very helpful response Austim.

This gives me the information needed to proceed with the project.