I am performing a project that requires addition of metric measurements to standards that now are all US.
The concrete mix designs are per AISC greenbook - in the form:
520-C-2500 (520=lb cement "c"=aggrgate size 2500=psi).
The new designation will be metric in the form (I found this formula in a municipality requirement):
310 kg/M(cubed) C 20 MPa
My question is, the conversions do not seem right.
First, I don't know what the M(cubed) is, so I don't know how to crank it in.
Secondly, 2500 psi does not convert to 20 MPa (megpascal).
I may be way off base, and am unfamiliar with this discipline.
Can anyone help clarify for me? Thanks so much...
The concrete mix designs are per AISC greenbook - in the form:
520-C-2500 (520=lb cement "c"=aggrgate size 2500=psi).
The new designation will be metric in the form (I found this formula in a municipality requirement):
310 kg/M(cubed) C 20 MPa
My question is, the conversions do not seem right.
First, I don't know what the M(cubed) is, so I don't know how to crank it in.
Secondly, 2500 psi does not convert to 20 MPa (megpascal).
I may be way off base, and am unfamiliar with this discipline.
Can anyone help clarify for me? Thanks so much...