Is there any statement in B31.4 that cite the two additional joint shall be inspected when the result of a joint girth weld reveal "rejected"?
This is a flowline with hydrocarbon services. RT was performed by 10% randomly.
 
Refer to API 1104. B31.4 434.8.5(b)sends you there....

The APIGUY....
 