Sep 28, 2009 #1 dursosono Materials Joined Aug 6, 2008 Messages 59 Location ID Is there any statement in B31.4 that cite the two additional joint shall be inspected when the result of a joint girth weld reveal "rejected"? This is a flowline with hydrocarbon services. RT was performed by 10% randomly.
Is there any statement in B31.4 that cite the two additional joint shall be inspected when the result of a joint girth weld reveal "rejected"? This is a flowline with hydrocarbon services. RT was performed by 10% randomly.
Oct 12, 2009 #2 apiguy Mechanical Joined Mar 5, 2002 Messages 116 Location US Refer to API 1104. B31.4 434.8.5(b)sends you there.... The APIGUY.... Upvote 0 Downvote