I have a condition where a 1/4" fillet weld has already been made. Now, a 5/16" fillet weld is required. Is it acceptable to just ad the additional 1/16" of weld?

Thanks!
 
Replies continue below

Recommended for you

Hi bsh117

You don't say how thick your metal components are, but your fillet weld size cannot exceed the thickness of the smallest section within the joint.

Regards

desertfox
 
Sorry, I didn't mention the thickness because they are ample size for a 5/16" weld...5/8" plates.
 
I have a condition where a 1/4" fillet weld has already been made. Now, a 5/16" fillet weld is required. Is it acceptable to just ad the additional 1/16" of weld?

Yes, provided you add filler metal to make the existing fillet legs equal in size for a 5/16" weld.

 
Also remember to have the initial weld properly cleaned before adding new filler metal.
 
There is no maximum fillet weld size in a T joint.

Hg

Eng-Tips policies: faq731-376
 