Table 4.2.1 in ACI 318-08 lists four "F" category exposure classes. It appears that if the top of an exterior foundation is above the frost line, then the concrete in that foundation must be at least 4500 psi (per table 4.3.1) and must be air entrained (per table 4.4.1). We have always air entrained our foundations, however we have previously always used 3000 psi concrete for below grade foundations. It appears that ACI 318-08 is now mandating a minimun compressive strength of 4500 psi for all foundations when the tops of the foundations are above the frost line.
I would like to get the opinions of other engineers. Is everyone now specifying 4500 psi concrete for their foundations? This requirement seems to be solving a problem that I never knew existed.
Thanks!
I would like to get the opinions of other engineers. Is everyone now specifying 4500 psi concrete for their foundations? This requirement seems to be solving a problem that I never knew existed.
Thanks!