I'm working on a few new products that will be used as automotive accessories, think canoe racks and things of that sort.
The designs we have are good, but the material suggested by our factory is entirely too expensive. They've suggested PC (didn't specify yet what specific type). We need a plastic material that will have good UV resistance and color fastness, and also needs to mate well with neoprene (our padding). With SolidWorks, I used a force of 1.5x larger than what we'll list as the maximum allowable on the product, and got the largest Von Mises stress to be 1001.7psi. The PC that I think they're using lists a yield strength of well over that.
Can anybody suggest a plastic that will have good UV resistance/color fastness, and will be strong enough for this application? I can find the strength properties for plastics relatively easy, but the UV properties are harder to come by. Many of these plastics have low resistance to UV in their raw form, but can be treated to attain acceptable UV resistance. The problem is I'm having trouble finding products that can and can't be treated for UV to an acceptable level.
PC is 2, 3, even 4x more expensive than many other commonly used plastics, and we've got to cut the price on the material. Any suggestions for plastics that can be treated for UV resistance and have good color fastness would really help out. Thanks guys
The designs we have are good, but the material suggested by our factory is entirely too expensive. They've suggested PC (didn't specify yet what specific type). We need a plastic material that will have good UV resistance and color fastness, and also needs to mate well with neoprene (our padding). With SolidWorks, I used a force of 1.5x larger than what we'll list as the maximum allowable on the product, and got the largest Von Mises stress to be 1001.7psi. The PC that I think they're using lists a yield strength of well over that.
Can anybody suggest a plastic that will have good UV resistance/color fastness, and will be strong enough for this application? I can find the strength properties for plastics relatively easy, but the UV properties are harder to come by. Many of these plastics have low resistance to UV in their raw form, but can be treated to attain acceptable UV resistance. The problem is I'm having trouble finding products that can and can't be treated for UV to an acceptable level.
PC is 2, 3, even 4x more expensive than many other commonly used plastics, and we've got to cut the price on the material. Any suggestions for plastics that can be treated for UV resistance and have good color fastness would really help out. Thanks guys