Hi,
I have a question about material SA/A335Gr.P91.
Before, we use SA/A335Gr.P91 for boiler main steam piping.
But this year, this material separate to SA/A335Gr.P91 TYPE1 & SA/A335Gr.P91 TYPE2.
Only can find some composition is different but no any further information about allowable stress(SEC II-D) & welding (SEC IX)
I'll very appreciate if there is any information for me to reference.
Thanks

Arstine
 
Replies continue below

Recommended for you

You will want to reference ASME Code Case 2864-1.

The maximum allowable stresses do change slightly above 1000 F

The devil is in the details; she also wears prada.
 
Hi,

Thanks for reply
I'vd check code case (ASME BPVC.CC.BPV-2019), I only find "Case 2864", there is no Case 2864-1.
Could you tell me where to download such information
Thanks

Arstine
 
Code Cases are not for download. More info on getting a copy.
The -1 in 2864-1 indicates a revision of 2864, however I wasnt able to locate this revision, it seems 2864 is current.
 
hi

The code case 2864 is ASME 2015.
P91 TYPE1/2 is shown in ASME 2019, so I think 2865-1 should be a new revision of code case.
But i just cant find it.
Thanks

Arstine
 
2864-1 is in the 2019 Code Cases for Boiler and Pressure Vessels. You will need to purchase 2019 Code Cases.

The devil is in the details; she also wears prada.
 
I have the 2019 edt of BPV CC, and mines only lists CC2864:
2864_atuh1v.png


The link I proivided doesnt show rev 1 either. Are you on an update cycle that may have recently issued this revision, whereas the pdf on the website isnt fully up2date yet?
 
XL83NL said:
Are you on an update cycle that may have recently issued this revision, whereas the pdf on the website isnt fully up2date yet?

Code Case 2864-1 was approved June 2019, and is found in Supplement 2 of the 2019 Code Cases. It is possible that Supplement 2 was recently released.

The devil is in the details; she also wears prada.
 
2864-1_rtp3jg.png


The devil is in the details; she also wears prada.
 
From what I can find, Supplements 1 and 2 have been active (released) since July 2019.

The devil is in the details; she also wears prada.
 
OK, ill dig deeper then to see what Im missing. Thanks for the update!
 
dear sir
I got the solution from IHS and get the code case supplements 2.
But here comes other question
The ASME BPVC.II.D.C-2019 show SA335P91 allowable is still different to code case 2864-1 table 3/3M
which one it type1 or type2

image_higbop.png
 
Table 3 of Code Case 2864-1 is for Type 2.

If you look at the chemistry requirements of Table 1, and compare them to the chemistry requirements from SA-335 of Type 2, they are the same. The code case tells you to use Table 3 for chemistries that meet Table 1.

The devil is in the details; she also wears prada.
 