Hi Guys,
I am looking at using A333 Gr6 for a low temp duty, but the equipment is made in Sch 160 pipe to PD5500 vessel code and the computed impact test temperature requirment is -77 Deg C, that standard test temperature for the material is somewhat lower.
Can anyone help me with some experience of doing impact testing at this low temperature as to whether or not you get sufficient impact values or would I be wasting my money on the tests by chasing a result that I cannot get.
Max
I am looking at using A333 Gr6 for a low temp duty, but the equipment is made in Sch 160 pipe to PD5500 vessel code and the computed impact test temperature requirment is -77 Deg C, that standard test temperature for the material is somewhat lower.
Can anyone help me with some experience of doing impact testing at this low temperature as to whether or not you get sufficient impact values or would I be wasting my money on the tests by chasing a result that I cannot get.
Max