Oct 9, 2008 #1 wfn217 Chemical Joined Aug 11, 2006 Messages 101 Location US Has anyone encountered A325 bolts from China with red stains. Do you know anything about what is causing this problem?
Has anyone encountered A325 bolts from China with red stains. Do you know anything about what is causing this problem?
Oct 9, 2008 #2 ctopher Mechanical Joined Jan 9, 2003 Messages 17,519 Location USA, CA Not using US material specs. I have encountered this before, all parts were scrapped each time. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion Upvote 0 Downvote
Not using US material specs. I have encountered this before, all parts were scrapped each time. Chris SolidWorks/PDMWorks 08 3.1 AutoCAD 08 ctopher's home (updated Aug 5, 2008) ctopher's blog SolidWorks Legion
Oct 11, 2008 #3 dinjin Mechanical Joined Jun 15, 2008 Messages 336 When and if your source is unreliable, I would test a number of these bolts to ensure that they are or meet the specs of A325 bolts. Upvote 0 Downvote
When and if your source is unreliable, I would test a number of these bolts to ensure that they are or meet the specs of A325 bolts.
Oct 17, 2008 #4 chicopee Mechanical Joined Feb 15, 2003 Messages 6,199 Location US I don't think these bolts are used on DOT projects. Last time we got a batch from Canada and CT DOT made us get rid of them eventought they were to anchor railings on top of parapet walls. Upvote 0 Downvote
I don't think these bolts are used on DOT projects. Last time we got a batch from Canada and CT DOT made us get rid of them eventought they were to anchor railings on top of parapet walls.
Oct 21, 2008 #5 HeviiGuy Mechanical Joined Oct 18, 2007 Messages 69 Location US Perhaps they're melamine-laced ;-) Ciao, HevïGuy http://www.heviitech.com Upvote 0 Downvote