Has anyone encountered A325 bolts from China with red stains. Do you know anything about what is causing this problem?
 
Replies continue below

Recommended for you

When and if your source is unreliable, I would test
a number of these bolts to ensure that they are or
meet the specs of A325 bolts.
 
I don't think these bolts are used on DOT projects. Last time we got a batch from Canada and CT DOT made us get rid of them eventought they were to anchor railings on top of parapet walls.
 