Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

a question about boiler's thickness 4

Status
Not open for further replies.

stonetech

Mechanical
Nov 3, 2006
29
There is a question " what would you do if you find for a boiler the leg (shell)'s thickness is not big enough?" Could you please help me with this question?
 
Replies continue below

Recommended for you

You mean not thick enough? Can you please come back with more specific information as to the type of boiler and your actual data (wall thickness and area affected)?
 
stonetech:

Mud Leg: perhaps?

Will the boiler still blowdown or is it packed solid?
Is it corroded from the outside or inside?
If it looks like "button-tuck" upholstery its time to replace.
A scab patch is not a fix.
 
What, you don't like the responses you got in the Piping & Fluid Mechanics thread you started.
 
Sorry for the late reply. In fact, this is a question asked during an interview. I don't have other details. I don't know how to answer it. That's the reason why I put it here. Anyway, Thank you everyone here.
 
Status