As a generalization with dissimilar stainless steels, the filler metal composition will tend toward that of the higher alloy base metal, or sometimes even higher.
Some welding development will be necessary here. Which just means trial welds with two or three fillers.
"Everyone is entitled to their own opinions, but they are not entitled to their own facts."