I have a part, 8620H, with an M20x1.5 OD thread on it. The part is to be machined and then quenched to 980MPA. It states the thread must not be hardened.
This isnt really a case depth type thing, I thought quenching was a metallurgical transformation (martensite?). Is there a level at which the hardening decreases?
Does anyone have experience with this type of situation?
The cross section is R20mm (.79) and about the same in length.
Thanks,
Tyler.
This isnt really a case depth type thing, I thought quenching was a metallurgical transformation (martensite?). Is there a level at which the hardening decreases?
Does anyone have experience with this type of situation?
The cross section is R20mm (.79) and about the same in length.
Thanks,
Tyler.