RAJMETALLURGY
Materials
Grade :4D/4C/60K
Tensile strength fail
Required value: 690 MPa min, but actual value: 664.62 MPa
Heat Treatment: Quecnch @ 930, 4 hrs soak & Tempered @ 660 Deg C 5 hrs soak.
What is the reason for tensile failure.
Tensile strength fail
Required value: 690 MPa min, but actual value: 664.62 MPa
Heat Treatment: Quecnch @ 930, 4 hrs soak & Tempered @ 660 Deg C 5 hrs soak.
What is the reason for tensile failure.