Hi,
I have read some information about the differences between 316L and 316Ti performances at high temperatures but I have some doubts yet. In our application, we have a kind of table made from a tube welded to a plate. That table is going to be at a high-temperature ambient (around 600 ºC) and normal air. Attending to the corrosion resistance, weldability and cost, what are the differences between 316L and 316Ti?
I have to say that we are from Europe, where the 316Ti is more common than in the USA.
Thanks.
I have read some information about the differences between 316L and 316Ti performances at high temperatures but I have some doubts yet. In our application, we have a kind of table made from a tube welded to a plate. That table is going to be at a high-temperature ambient (around 600 ºC) and normal air. Attending to the corrosion resistance, weldability and cost, what are the differences between 316L and 316Ti?
I have to say that we are from Europe, where the 316Ti is more common than in the USA.
Thanks.