All materail experts, I got a deviation request form supplier, pelase help to see if that is accepatble or not:
Our valve supplier is proposing the cast version of 316H (Material Designation A351-CF8M high temperature casting material, which will meet the H grade specified) in lieu of F316H forging for the automated on-off valve bodies.
Our Piping Material Class Specification states 316H body required for valves in this severe high-temp service, but does not specify whether or not cast bodies are acceptable.
The supplier states A351-CF8M cast valve body is what is currently available to meet our delivery schedule.
Will that be acceptable for the cast valve body ? This is for 1450 degF/ 60 psig service with catalyst flowing that erosion is the concern.
Our valve supplier is proposing the cast version of 316H (Material Designation A351-CF8M high temperature casting material, which will meet the H grade specified) in lieu of F316H forging for the automated on-off valve bodies.
Our Piping Material Class Specification states 316H body required for valves in this severe high-temp service, but does not specify whether or not cast bodies are acceptable.
The supplier states A351-CF8M cast valve body is what is currently available to meet our delivery schedule.
Will that be acceptable for the cast valve body ? This is for 1450 degF/ 60 psig service with catalyst flowing that erosion is the concern.