Wondering if anyone here has had any experience with welding 310 material to G-30 hastelloy material. If so, what SMAW filler metal did you use?

Thanks,
Robert
 
qcrobert;
My question back to you is what is the intended service of this dissimilar metal weld joint? Corrosion at elevated temperature?
 
It is for elevated temperature to weld 1/4" 310 angle clips (that hold insulation) to G-30 Hastelloy base metal.

My thoughts are using SMAW process with 3/32" dia electrodes (field install) and Hastelloy X filler metal.

Do you concur?
Robert
 