I know that this is probably a pretty basic question, however, I have just started to work with the Pressure Vessel Code. Where are the stress tables for 304L located?
 
Replies continue below

Recommended for you

I was able to locate them via the online tables.
 
gmarken (Mechanical):

For material occurs in ASME II-D (table 1A) tables more than once be careful of note G5 (as in table 1a Notes) especially when dealing with austenitic SS like 304.