cdnprodigy
Materials
I have a question regarding the compressibility of a nanodiamond. It is regarding the steric accuracy of a diamond probe surface.
Assuming a block of singly nucleated nanodiamond 100 X 100 X 100 nm. Assuming a section *magically* cut out of the middle measuring 75 X 75 X 1 nm. The goal is to press the sides of the diamond block and have the cutout inner surface faces touch. My question is, would the diamond fracture before the opposing cutout surfaces touched?
I think this is basically a three point bending test of a very small chunk of diamond measuring 75 X 75 X 49.5 nm. Could the diamond be bent 4 or 5 angstroms along its 49.5 nm thickness before fracturing? I'm sure there is an equation to plug in numbers, but I don't yet know what it is. Thx.
Assuming a block of singly nucleated nanodiamond 100 X 100 X 100 nm. Assuming a section *magically* cut out of the middle measuring 75 X 75 X 1 nm. The goal is to press the sides of the diamond block and have the cutout inner surface faces touch. My question is, would the diamond fracture before the opposing cutout surfaces touched?
I think this is basically a three point bending test of a very small chunk of diamond measuring 75 X 75 X 49.5 nm. Could the diamond be bent 4 or 5 angstroms along its 49.5 nm thickness before fracturing? I'm sure there is an equation to plug in numbers, but I don't yet know what it is. Thx.