Dear welding engineering connections

Is there any available provision for permitting sub size Charpy impact specimen for welding consumable mechanical testing - SFA5.18 ER70S-6?

Thanks in advance
 
Theoretically yes, as the required testing standard, AWS B4.0, commences the requirement for test piece dimensions with "Unless otherwise specified...". A classic specification writing error, but nevertheless, it conveys that the requirement is not actually fixed.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 