Dear welding engineering connections
Is there any available provision for permitting sub size Charpy impact specimen for welding consumable mechanical testing - SFA5.18 ER70S-6?
Thanks in advance
Is there any available provision for permitting sub size Charpy impact specimen for welding consumable mechanical testing - SFA5.18 ER70S-6?