Dec 7, 2017 #1 Mous1747 Mechanical Joined Apr 11, 2013 Messages 91 Location US why it's not common or industry standard to 3 mil ENP on a 316 ball? but
Jan 27, 2018 #2 mk3223 Mechanical Joined Feb 4, 2006 Messages 1,488 Location US IMO, there is no need to have ENP coating on 316SS, which is to provide a corrosion resistant surface as 316SS itself. Upvote 0 Downvote
IMO, there is no need to have ENP coating on 316SS, which is to provide a corrosion resistant surface as 316SS itself.
Jan 28, 2018 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,944 Location GB Why should it be a standard? It's generally for tribological purposes rather than corrosion control, and is a subjective materials selection. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
Why should it be a standard? It's generally for tribological purposes rather than corrosion control, and is a subjective materials selection. Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer.