16'' sch 80 TP 316/316L Stainles Steel pipe has been cutted 12 mm short an we do not have any additional material..So that i would like to make welding filling with the ER 316 L welding wire or suitable electrode from pipe end to provide at least 10 mm filling in order the get requested pipe dimension. As i know it is call as bathering..is there any part of ASME spec?
What is the allowlable limit this option?
 
It's called "buttering" and the limit on thickness of the "butter" layer should be the maximum thickness of weld deposit qualified by the PQR. Typically 2 times the deposit thickness used in the procedure qualification.
 