roberthathaway
Materials
We have run into an interesting failure with this thread that is at the end of a small hydraulic cylinder. 90% of the failure is brittle cleavage, however 10% at thread root initiation is dimple rupture. We believe that the cyclinder experience impact loading, but why would it initiate through a ductile mode, why not brittle fracture across then entire cross section. The fastener is at 23 HRC but is not heat treated and the threads are cut. Any ideas as fas as why a ductile failure would progress into brittle would be appreciated.