What is the recommended welding rod material to MIG or TIG these materials together? Ray Reynolds
Senior Designer
Read: faq731-376
"Probable impossibilities are to be preferred to improbable possibilities."
 
Replies continue below

Recommended for you

A typical filler metal would be ER309L, but this can vary based on the type of application, PHWT if any, intended use, etc.
 