Hi, our company has a Mitsubishi CO2 laser, model 3015LVP-40CFX. I try to cut 0.047” galvanized material. What cutting condition can I use? Thanks
 
you can use stainless steel condition for the same thickness but cut your speed in half. there will be burr on the bottom but it will cut
 