Hi, our company has a Mitsubishi CO2 laser, model 3015LVP-40CFX. I try to cut 0.047” galvanized material. What cutting condition can I use? Thanks
 
Replies continue below

Recommended for you

you can use stainless steel condition for the same thickness but cut your speed in half. there will be burr on the bottom but it will cut
 