Hi All

Prepared test piece to send for mechanical testing for materia Api 5l x65 psl2 which mechanical test required,how many and dimension

Thanks

 
Replies continue below

Recommended for you

You're asking us to do your work for you? The answers are in the standard.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
The new API 5L aligned with the ISO 3183 requires different scopes of testing depending on the utilisation of this pipe!
And the testing also depends on the WT and OD...