hi everyone,

anyone could please help me to understand the min allowance temperature for
a193 b7 - some stated -29degC while some -40degC.
a193 b7m - some stated -29degC while some -48degC.
the maximum temp is consistent at 400degC.
i'm confused

thanks a lot.
 
Replies continue below

Recommended for you

So that I don't have to look up A193 or rely too much on my memory, what is 'allowance temperature'?

p.s., punctuation would enhance your reputation as a communicator.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
In the valve world, the general understanding for SA 193 Gr.B7 low temp limit is -29 Deg.C
Below this, an impact tested steel such as SA 320 Gr.L7 is used dependent on application.

Per ISO-4126, only the term Safety Valve is used regardless of application or design.
 
What the others said. Furthermore, the applicable code of construction will probably have final say in this.