INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

1018 CD Steel

1018 CD Steel

1018 CD Steel

(OP)
What is the yield shear stress for 1018CD steel?
Thanks.
Replies continue below

Recommended for you

RE: 1018 CD Steel

cadet,

Go to www.matweb.com

Under Quik search type in: AISI 1018

RE: 1018 CD Steel

Cadet

Suggest you follow eureka,s good advice and visit www.maweb.com because that will show you the added spec details you need for SAE 1018.  

But that site won't give you the yield shear stress that
you have asked for. The Metals Handbook (9th edition) pp 160/161 gives the distribution of mechanical properties for most of the different SAE 1018 specs.

Hope you'll find what you need there.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close