Our need is to paint or powdercoat onto polypropylene to acheive an aluminum finish. Any direction as to a vendor or process to do these parts?
 

Ask a capable paint manufacturer to formula a 2K Urethane (paint) system with a compatable Aluminum flake pigment.

Hold on to your butt when he begins to talk price per gallon.
 