zonatile

Status
Not open for further replies.

DCEB

Structural
Joined
Mar 22, 2012
Messages
2
Location
US
thread507-232131

I read this earlier thread and we have just come upon Zonatile that failed in an industrial building. I was wondering if anyone has any info on it
 
Please describe the material as the term "Zonotile" might be a misspelled term as noted in the other thread. Please give the age of the building and the manifestation of failure. Photos would be helpful as well.
 
DCEB...thanks. Zonatile was manufacturered by the Zonolite Company which was purchased by W.R. Grace in the early 1960's. They apparently dropped Zonatile from their product line 4 or 5 years later.

I'm wondering if it did not compete well with cast-in-place gypsum and Tectum decks that were popular in that era.

The info you have is probably as good as you'll get!
 