PSUengineer1
Structural
An internet search yields limited product information on Zonatile precast concrete roof decks. The planks are precast concrete about 18"x36"x3". Reinforcing is 2x4-12/12 galvanized wire reinforcement, I assume placed in the tension zone (bottom) of the plank. Is there also top reinforcement typically in this system? From what I could find, the planks carry up to 50 psf superimposed. Any other data on this product would be appreciated. Thanks.