The words sacrificial protection springs to mind, if you have anything metallic in the pool higher up in the recation talbe, ie steel, etc thenthe zinc will sacrifice itself to protect the steel. hence galvanised steel. what you will create is like a battery with with the flow from zinc to parent metal. that is unless your swinning pool is made of gold, silver or platinum.