Dec 21, 2011 #1 ToadJones Structural Joined Jan 14, 2010 Messages 2,299 Location US MBMA or anyone have literature for designing light gauge Z purlins for biaxial bending?
Dec 21, 2011 #2 SteveGregory Structural Joined Jul 18, 2006 Messages 554 Location US Check the current AISI Cold Formed Steel Design Manual. Upvote 0 Downvote