JG MechEng
Mechanical
I have been asked by a client to rerate heater tubes to 1375 deg F and 890psi. Spent a fair amount of time trying to find yield strength data for 9 chrome at that elevated temperature. Also, API 530 larson miller parameter tables stop at 1300 deg F. Looking for some guidance on locating material data for the material to see if it’s even possible to make work. I do not want to get into a code discussion, this is not a code state and the client is willing to accept those risks.