Hi All,
I am working on a plastic material with YS = 30MPa,Yield Strain is 2.5%. Modulus is 3400 MPa. I got a stress-strain data (engineering stress-strain) and I want to calculate plastic strain.
The modulus given in the spec is initial modulus and I measured 0.2% from the stress-strain curve, the yield stress/ strain is actually less than YS (30MPa) and Yield Strain (2.5%).
I am not sure if I should assume the plastic deformation starts at 0.2% or 30MPa?
Thanks!
I am working on a plastic material with YS = 30MPa,Yield Strain is 2.5%. Modulus is 3400 MPa. I got a stress-strain data (engineering stress-strain) and I want to calculate plastic strain.
The modulus given in the spec is initial modulus and I measured 0.2% from the stress-strain curve, the yield stress/ strain is actually less than YS (30MPa) and Yield Strain (2.5%).
I am not sure if I should assume the plastic deformation starts at 0.2% or 30MPa?
Thanks!