Do anyone know the yield strength for "AMS 5344 17-4PH", "C.S SA-36" and "St 1550" at temp. 20 and 100 20degrees Celsius?
 
For 17-4PH
0,2% Yield stress
at 100°C
>= 880 N/mm²
at 150°C
>= 830 N/mm²
at 200°C
>= 800 N/mm²
at 250°C
>= 770 N/mm²
at 300°C
>= 750 N/mm²
This is from Stahlschlussel. Please provide more information about the other steels.
 