For 17-4PH
0,2% Yield stress
at 100°C
>= 880 N/mm²
at 150°C
>= 830 N/mm²
at 200°C
>= 800 N/mm²
at 250°C
>= 770 N/mm²
at 300°C
>= 750 N/mm²
This is from Stahlschlussel. Please provide more information about the other steels.
 