Dec 7, 2005 #1 Rikki123 Mechanical Joined Dec 7, 2005 Messages 1 Location SE Do anyone know the yield strength for "AMS 5344 17-4PH", "C.S SA-36" and "St 1550" at temp. 20 and 100 20degrees Celsius?
Do anyone know the yield strength for "AMS 5344 17-4PH", "C.S SA-36" and "St 1550" at temp. 20 and 100 20degrees Celsius?
Dec 7, 2005 #2 adyonel Materials Joined Aug 25, 2005 Messages 18 Location US For 17-4PH 0,2% Yield stress at 100°C >= 880 N/mm² at 150°C >= 830 N/mm² at 200°C >= 800 N/mm² at 250°C >= 770 N/mm² at 300°C >= 750 N/mm² This is from Stahlschlussel. Please provide more information about the other steels. Upvote 0 Downvote
For 17-4PH 0,2% Yield stress at 100°C >= 880 N/mm² at 150°C >= 830 N/mm² at 200°C >= 800 N/mm² at 250°C >= 770 N/mm² at 300°C >= 750 N/mm² This is from Stahlschlussel. Please provide more information about the other steels.
Dec 7, 2005 #3 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA 17-4 aged at what temp? to what properties? You need a starting point. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
17-4 aged at what temp? to what properties? You need a starting point. = = = = = = = = = = = = = = = = = = = = Corrosion, every where, all the time. Manage it or it will manage you. http://www.trent-tube.com/contact/Tech_Assist.cfm
Dec 7, 2005 #4 adyonel Materials Joined Aug 25, 2005 Messages 18 Location US 17-4 aged at 550 Celsius. Upvote 0 Downvote