Dec 2, 2008 #1 dummiboi Mechanical Joined Jul 3, 2006 Messages 14 Location US Hi, Where can I find data on the yield strength and tensile strength of S31600 at around 258F? Thanks, Jesse
Hi, Where can I find data on the yield strength and tensile strength of S31600 at around 258F? Thanks, Jesse
Dec 2, 2008 1 #2 Maui Materials Joined Mar 5, 2003 Messages 1,952 Location US You can find the yield strength data that you requested here: http://www-ferp.ucsd.edu/LIB/PROPS/PANOS/ss.html Maui Upvote 0 Downvote
You can find the yield strength data that you requested here: http://www-ferp.ucsd.edu/LIB/PROPS/PANOS/ss.html Maui
Dec 2, 2008 1 #3 JoeTank Structural Joined Oct 28, 1999 Messages 1,133 Location US ASME SECTION II, Subpart D (Allowable Stresses) has the exactly the info you need. Joe Tank Upvote 0 Downvote
Dec 2, 2008 1 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Another option, if the material is in a solution annealed condition, and you know the product form, you can go to ASME B&PV Code, Section II, Part D, Table U and Table Y-1. Upvote 0 Downvote
Another option, if the material is in a solution annealed condition, and you know the product form, you can go to ASME B&PV Code, Section II, Part D, Table U and Table Y-1.
Dec 3, 2008 Thread starter #5 dummiboi Mechanical Joined Jul 3, 2006 Messages 14 Location US Thanks everyone! Upvote 0 Downvote